ZHENG Qingshuang, CHEN Shenglin, QIAO Ang, WANG Mitang, TAO Haizheng. Crystallization Behavior and Mechanical Properties of Zinc-Containing Yttrium Aluminosilicate Glasses[J]. Journal of the Chinese Ceramic Society, 2024, 52(8): 2495

Search by keywords or author
- Journal of the Chinese Ceramic Society
- Vol. 52, Issue 8, 2495 (2024)
Abstract
Methods On the basis of the glass composition 22Y2O3·19Al2O3·59SiO2, a series of glasses with varying compositions,2xZnO·22Y2O3·(19–x)Al2O3·59SiO2 (2x=0, 3, 6, 12, 18, in mole), were obtained by gradually replacing Al2O3 with ZnO at a ZnO:Al2O3 ratio of 2:1. The glasses were subjected to a nucleation temperature (Tg+30 ℃) heat treatment for 3 h, followed by ramping to the crystallization peak temperature (Tc) and holding for 2 h to obtain glass ceramics for testing. Characteristic temperatures of the glasses were determined using DSC at a heating rate of 10 K/min. The glass ceramics, after fine polishing, were etched for 60 s in a 4% HF solution (volume fraction) and then subjected to SEM testing. Vickers hardness of the samples was measured under a 2.94 N load. Fracture toughness (KIc) of the samples was determined under the ASTM C-1421-01b standard
Results and discussion As the amount of ZnO gradually increases, the glass transition temperature (Tg) and Tc of the glass decrease progressively. The addition of ZnO reduces both Tg and Tc of the YAS glasses, which is advantageous for lowering the sealing temperature when used in conjunction with SiC ceramics. XRD patterns, SEM images, and EDS patterns confirm that the mechanism for the precipitation of y-Y2Si2O7 in 22Y2O3·19Al2O3·59SiO2 glass belongs to crystallization through phase separation. After the addition of ZnO to YAS glass, nearly spherical grains are precipitated, and the distribution of grains becomes more uniform. With increasing ZnO content, the grain size gradually decreases. The addition of ZnO has a minor impact on the hardness and density of both YAS glass and glass-ceramics. However, a significant improvement is observed in the fracture toughness of the glass ceramics,showing a 65% increase for the glass ceramic containing 18% ZnO compared to the YAS glass ceramic. In glass ceramics formed through phase separation and grain growth, both the size and distribution of grains are uneven. Cracks propagate in a straight-line manner, resulting in longer crack lengths under the same load. In contrast, when cracks propagate in glass ceramics with similar and evenly distributed grain sizes, numerous circumferential cracks around grains occur, leading to increased energy consumption during the crack propagation process and resulting in relatively shorter crack propagation distances.
Conclusions As ZnO gradually replaces Al2O3, both the Tg and Tc of YAS glasses decrease. This leads to reduce the sealing temperature when used as sealing materials. With the addition of ZnO, the crystal phases deposited from the YAS glasses transitions from only the y-Y2Si2O7 grains to two phases, i.e., ZnAl2O4 and y-Y2Si2O7. The content of precipitated ZnAl2O4 phase increases with the gradual introduction of ZnO. Although no significant increase in hardness was observed following the compositional change from 0 to 18% of ZnO (in mole), a distinct enhancement of about 1 GPa in hardness after crystallization occurs for the glass with ZnO.Despite a decrease in KIc of YAS glass from 0.82 MPa·m0.5 to 0.71 MPa·m0.5 with the addition of ZnO, the prepared glass ceramics with 18% ZnO (in mole) shows a significant enhancement of KIc, reaching a maximum value of 1.92 MPa·m0.5. The microscopic mechanisms of this enhancement was then revealed by further investigation using SEM.

Set citation alerts for the article
Please enter your email address