[3] Y XU, W ZHANG. Numerical modelling of oxidized microstructure and degraded properties of 2D C/SiC composites in air oxidizing environments below 800 ℃. Materials Science and Engineering(2011).
[4] A LACOMBE, T PICHON, M LACOSTE. High temperature composite nozzle extensions: a mature and efficient technology to improve upper stage liquid rocket engine performance. 43rd AIAA/ASME/SAE/ASEE Joint Propulsion Conference & Exhibit, Cincinnati.
[7] M C HALBIG, J D MCGUFFIN-CAWLEY, A J ECKEL et al. Oxidation kinetics and stress effects for the oxidation of continuous carbon fibers within a microcracked C/SiC ceramic matrix composite. Journal of the American Ceramic Society(2008).
[9] X CHEN, Z SUN, P CHEN et al. Modeling thermal expansion behavior of 2.5D C/SiC composites in air oxidizing environments between 400 ℃ and 800 ℃. Applied Composite Materials(2020).
[10] H MEI, Y TAN, P CHANG et al. Simplified approach to study oxidative damage of C/SiC composites induced from notch defects. Ceramics International(2019).
[11] F LAMOUROUX, G CAMUS, J THEBAULT. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: I. experimental approach. Journal of the American Ceramic Society, 8:, 2049(1994).
[12] F LAMOUROUX, R NASLAIN, J JOUIN. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: II, theoretical approach. Journal of the American Ceramic Society, 8:, 2058(1994).
[13] R M SULLIVAN. A model for the oxidation of carbon silicon carbide composite structures. Carbon(2005).
[14] C ZHAO, Z TU, J MAO. The dynamic thermophysical properties evolution and multi-scale heat transport mechanisms of 2.5D C/SiC composite under high-temperature air oxidation environment. Composites Part B(2023).
[15] J DING, Z SUN, X CHEN et al. A progressive oxidative damage model of C/SiC composites under stressed oxidation environments. Applied Composite Materials(2021).
[17] P CHEN, X NIU, X CHEN et al. Modeling the failure time and residual strength of C/SiC composites under stress-oxidation environment. Transactions of the Indian Ceramic Society(2020).
[18] C ZHAO, Z TU, J MAO. Thermal-oxidation coupled analysis method for unidirectional fiber-reinforced C/SiC composites in air oxidizing environments below 1000 ℃. International Communications in Heat and Mass Transfer(2023).
[19] A J ECKEL, J D CAWLEY, T A PARTHASARATHY. Oxidation kinetics of a continuous carbon phase in a nonreactive matrix. Journal of the American Ceramic Society(1995).
[20] E J OPILA, J L SERRA. Oxidation of carbon fiber-reinforced silicon carbide matrix composites at reduced oxygen partial pressures. Journal of the American Ceramic Society, 7:, 2185(2011).
[21] Y XIANG, F CAO, Z PENG et al. Evolution of microstructure and mechanical properties of PIP-C/SiC composites after high- temperature oxidation. Journal of Asian Ceramic Societies(2017).
[22] F SU, P HUANG, J WU et al. Creep behavior of C/SiC composite in hot oxidizing atmosphere and its mechanism. Ceramics International(2017).
[23] S DRAWIN, M BACOS, J DORVAUX et al. Oxidation model for carbon-carbon composites. 4th Symposium on Multidisciplinary Analysis and Optimization, Cleveland.
[25] B E DEAL, A S GROVE. General relationship for the thermal oxidation of silicon. Journal of Applied Physics(1965).
[26] L FILIPUZZI, R NASLAIN, C JAUSSAUD. Oxidation kinetics of SiC deposited from CH3SiCl3/H2 under CVI conditions. Journal of Materials Science(1992).
[27] Y SONG, S DHAR, L C FELDMAN. Modified deal grove model for the thermal oxidation of silicon carbide. Journal of Applied Physics(2004).
[28] E N FULLER, P D SCHETTLER, J C GIDDINGS. New method for prediction of binary gas-phase diffusion coefficients. Industrial & Engineering Chemistry(1966).
[29] M KNUDSEN. The laws of molecular flow and of inner friction flow of gases through tubes. Journal of Membrane Science(1995).